Characteristics | Test Method | English | Metric |
Areal Weight | ASTM D3776 | 15.0 oz./sq. yd. | 510 gms./sq.m. |
Thickness | ASTM D1777 | 0.025 inches | 0.64 mm. |
Breaking Strength (lbs.) | |||
Warp | ASTM D5034 | 220 lbs. | 979 N |
Fill |
ASTM D5034 | 150 lbs. | 667 N |
Tear Strength (lbs.) | |||
Warp |
ASTM D1424 | 15 lbs. | 67 N |
Fill |
ASTM D1424 | 15 lbs. | 67 N |
Flame Resistance |
|||
After Flame (max.) |
ASTM D6413 | 2.0 seconds | 2.0 seconds |
Char Length (max.) |
ASTM D6143 | 4.0 inches | 10 cm. |
Radiant Reflectivity (min.) | MIL-C-24929A | 20 seconds | 20 seconds |
Thanks to its lower cost and heavier construction, this fabric is very popular for glove backs used in welding as well as in industrial garments and industrial gloves. Specifically, it is good in instances where there is high radiant heat and minor potential for molten metal splash.