Characteristics |
Test Method |
English |
Metric |
Areal Weight | ASTM D3776 | 5.3 oz./sq. yd. | 180 gms./sq. m. |
Thickness | ASTM D1777 | 0.006 in. | 0.15 mm. |
Breaking Strength | ASTM D5034 | ||
Warp | 100 lbs. | 445 N | |
Fill | 50 lbs. | 220 N | |
Tear Strength | ASTM D1424 | ||
Elmendorf Tear | |||
Warp | 2.0 lbs. | 9 N | |
Fill | 2.0 lbs. | 9 N | |
Flame Resistance | ASTM D6413 | ||
After Flame | 2.0 sec. | 2.0 sec. | |
Char Length | 1.0 in. | 2.54 cm. | |
Radiant Reflectivity | MIL-C-24929A | 10 sec. | 10 sec. |